Microhardness change on composite resin surface after treatment for 30 minutes Unit: VHN
Group | N | Treatment | △VHN |
|
---|---|---|---|---|
Before (0 min) | After (30 min) | |||
1 |
12 | 83.63±1.40 | 81.92±1.01 | ―1.71±0.57a |
2 |
12 | 83.57±1.41 | 72.10±1.57 | ―11.48±1.45d |
3 |
12 | 83.52±1.31 | 73.98±1.59 | ―9.54±1.15c |
4 |
12 | 83.52±1.20 | 74.30±0.41 | ―9.21±1.21c |
5 |
12 | 83.49±1.09 | 75.39±0.69 | ―8.10±0.92b |
6 |
12 | 83.64±0.92 | 75.51±0.72 | ―8.14±0.84b |
All values are mean±standard deviation.
*
**
a,b,c,dThe same letter indicates no significant difference by Duncun’s test at α=0.05.
Group: 1, mineral water; 2, carbonated beverage; 3, fermented milk; 4, fermented milk+3% Ca; 5, 2% NaF+fermented milk; 6, 2% NaF+(fermented milk+3% Ca).